Preparation: 120(48T) Mesh number ;65-75 degree Squeegee. For white and fluorescent color 20%,other color 10% 2% slow dry XG-866B-1 and fast dry XG-866B-2 can mix together for using. 0-20%    thinner is not necessary for hand printing 100℃- 120℃ for 6-10 seconds Silicone ink printing tips: 1. HD silicone/soft silicone    XG-866AH/XG-866AR        60G Fast dry catalyst            XG-866B-2        […]

10Dec 2021

1st : Filling bellow mixing moulding silicone ink together into the mould Moulding silicone  XG-360W 60G Silicone catalyst  XG-360WB 6G 10% Pigments              1.2-2.4G 2-4% 2nd: Get the hot melt paper on the silicone ink filled mould 3rd. Machine heat press including vacuum , venting and curing together ,this should get special machine with Vacuum funtion […]

20Nov 2021

Preparation: Mesh&Squeegee: 120(48T) Mesh number; 65-75 degree Squeegee. : Pigments added ratio:For white and fluorescent color 20%,other color 10% Catalyst mixing ratio:2% slow dry XG-866B-1 and fast dry XG-866B-2 ,hand printing to use fast dry catalyst and ,machine printing to use slow dry catalyst or slow dry catalyst and fast dry catalyst to mix together for using. Thinner XG-128A adding […]

12Nov 2021

G-15T+ &catalyst XG-15B Preparation: Mesh: 30-60(12T-24T) to make thick screen by emulsion.Can use Hollow aluminum screen. Pigments added ratio:4% Catalyst mixing ratio:2%  Thinner XG-128AH adding ratio:0-10%    thinner is not necessary Heating Temp and time: 150℃ -170℃ for 6-12 seconds , Heating time depends on drying temp. Silicone ink mixing tips: Printing silicone       XG-15T        50G Catalyst               XG-15B+       1 G  (2%) Pigment              XG-            2G  (4%) Silicone […]

28Oct 2021

Preparation: Mesh&Squeegee: 120(48T) Mesh number; 65-75 degree Squeegee. Pigments added ratio: For white and fluorescent color 20%, other color 10% Catalyst mixing ratio: 2% slow dry XG-866B-1 and fast dry XG-866B-2 can mix together for using. Thinner XG-128A adding ratio: 0-20%    thinner is not necessary for hand printing Flash cure temp: 100℃- 120℃ for 6-10 seconds Silicone ink printing tips: HD […]

12Oct 2021

Preparation: Mesh: 30-60(12T-24T) to make thick screen by emulsion. Better to use Hollow aluminum. Pigments added ratio: 2-4% Catalyst mixing ratio: 2%  Thinner XG-128AH adding ratio: 0-10%    thinner is not necessary Heating Temp and time: 120℃ -150℃ for 6-12 seconds, Heating time depends on drying temp. Silicone ink mixing tips: Printing silicone       XG-15A+        60G Catalyst               XG-15B+       1.2G  (2%) Pigment              XG-           1.2-2.4G […]

09Sep 2021

Preparation: Mesh&Squeegee: 120(48T) Mesh number ;65-75 degree Squeegee. Pigments added ratio:For white and fluorescent color 20%,other color 10% Catalyst mixing ratio:2% slow dry XG-866B-1 and fast dry XG-866B-2 can mix together for using. Silicone thinner XG-128A adding ratio:0-20%    Silicone thinner is not necessary for hand printing Heating Temp and time: cure temp :100℃- 120℃ for 6-10 seconds ,Drying temp :120℃- 140℃ for […]

16Jul 2021

Dipping Ink for Ropes & Tape, Shoelace Dipping Ink Tips Color effect to dip 2-4 times:  Dipping ink    XGF-5338/5338C     100G (5338C harder hand feel)  Color pigments                   2-4G    2-4%  Fixer        XGF-313            1-2G    1-2% Purified water                    5-20G   5-20%  If need glossy effect after color to dip Glossy Dipping Ink XGF-110L for 1 time: Glossy Dipping Ink  XGF-110L  100G   Fixer             XGF-313 […]

29Jun 2021
Conductive-silicone

Conductive Silicone for Conductive Gloves Printing Gloves Printing Conductive Ink Preparation: Mesh&Squeegee: 100-120(40-48T) Mesh number; 65-75 degree Squeegee. Catalyst mixing ratio:2%   Thinner XG-128A adding ratio:0-20% Heating Temp and time: Flash cure temp: 100℃- 120℃ for 6-10 seconds, Drying temp: 120℃- 130℃ for about 2 -3 minutes. Round Silicone for under printing for 2 times: Round silicone       XG-866A-2Y    50G Fast dry catalyst        XG-866B-2       1G    2% Silicone […]