1.TO mix with Solid sicone and transparent,ratio:10:1

2.Fix the screen, brush the concave and convex silica gel on the back of the mold, in order to separate the mold, the above is the convex groove, the below is the groove.

3.Silicone is printed on the cloth and then another cloth is pressed on top of it for pressing.

4.Pressing temperature:

On the temperature180℃~200℃

Lower temperature temperature : 80℃~100℃

Pressing time: 15 to 18 seconds