How to print supper smooth glossy silicone effectKey points of HD Glossy Silicone Ink Screen Printing:

1.To chose thick screen

2.For hairy fabric to heat press by heat press machine or iron after first time silicone printing for smooth effect.

Silicone ink is sticky when lift up the screen and heat all fabric hairy will stand up,if heat press then all fabriy hairy will lie flatand get smooth effect.First printing can not heat need to keep 100%wet before heat press.

3.For glossy silicone printing,after printing should waite bubbles out then to cure by lower temp like 100-110 degree.For

glossy silicone can printing 1-2 times,if two times printing can print wet on wet or heat then screen printing again.

HD glossy silicone ink printing process:Preparation

1.Mesh&Squeegee:120(48T)Mesh number;65-75 degree Squeegee.

2.Pigments added ratio:For white and fluorescent color 20%,other color 10%

3.Catalyst mixing ratio:2%slow dry XG-866B-1 and fast dry XG-866B-2 can mix together for using.Slow dry catasyt formachine printing.

4.Silicone thinner XG-128A adding ratio:0-20%Silicone thinner is not necessary for hand printing

5.Heating Temp and time:Flash cure temp:100℃-120℃ for 6-10 seconds ,Drying temp:120℃-140℃ for about 2-3 minutes.

Silicone ink printing tips:

1.HD silicone XG-866A/866AH for under coating and high density printing for 2-8 times:

HD silicone XG-866A/866AH 60G

Fast dry catalyst XG-866B-21.2G 2%

Silicone thinner XG-128AH Silicone thinner is not necessary for hand printing,5-20%is enough for machine

printing.Cure by temp of 120℃ 6-10 seconds.

If fabric with hairy or want to get more smooth effect kindly assist by heat press machine or iron after first time printing.After printing keep wet to heat press by temp 150-170 degree for 10-20 seconds.

2.Color effect silicone printing for 3-4 times:

HD silicone XG-866A/866AH 60G

Black color pigment XG-1026G For white and fluorescent color 20%,other color 10%Fast dry catalyst XG-866B-21.2G 2%If machine printing to use slow dry catalyst.Silicone thinnerXG-128AH Silicone thinner is not necessary for hand printing,5-10%is enough for machineprinting.Cure by temp of 120℃ 6-10 seconds.

3.Glossy silicone ink or matte silicone ink for top coating:

Glossy top coating for 1-2 times:

Glossy silicone ink XG-399-3 60G

Fast dry catalyst XG-866B-21.2G 2%It will be better to use slow dry catalyst XG-866B-1 and fast dry half and half.If for machine printing to use slow dry catalyst.

Silicone thinner XG-128AH Silicone thinner is not necessary for hand printing,5-10%is enough for machine printing.Cure by temp of 100-110℃ 10-25 seconds Have to get silicone bubbles out first ,try to use code wind to support and it will bebetter to use low temp by longer heating time.To avoid bubbles problem.