1.To mix with silicone and catalyst ,Printing 3 times ,Flash by

120 degree for 8-15 seconds

Soft silicone paste XG-866AR 100G

Fast dry catalyst XG-866B 2G

2.To mix with silicone and catalyst ,Printing 3 times ,Flash by 120 degree for 8-12 seconds

Soft foaming silicone XG-866ARP 200G

Fast dry catalyst XG-866B-2 4G

3.Couring by 150-160 degree for 1-2 minutes by tunnel drying oven