1.To mix with Silicone ,Catalyst and thinner ,Printing clear effect for under coating 2 times,Heating temp 120 degree

Elastic silicone XG-866A-LK 210G

Thinner XG-128AH 21G

Fast dry catalyst XG-866B-2 4.2G

2.Color pigment print to 2 times ,Heating temp 120 degree

Elastic silicone XG-866A-LK

Thinner XG-128AH 10-20%

Fast dry catalyst XG-866B-2 2%

Pigment 10%

3.Pulling printing for 1 time,Heating temp 120 degree