1.HD sillicone to mix with catelyst to print for under coating for 2 time ,heating by temp of 120 degree,the second time heat by press machine under 170-180 degree for 8-15 seconds
HD silicone XG-866A
Catalyst XG-866B-2 2%
2.Soft silicone mix with catalyst and red silicone pigments to print 20-30 times,flash by temp of 120 degree,Than black silicone pigment to print 3-4 times
Soft silicone XG-866ARP
Catalyst XG-866B-2 2%
Red silicone pigment 10%
Black silicone 10%
After finish to cure by 120-140 degree for 2-5 minutes