1.To mix with silcone and catalyst,Under coating for two times,Heating temp 120 degree.
HD silicone XG-866A 50%
Elastic silicone XG-866A-LK 50%
Catalyst XG-866B-2 2%
2.Color effect to print for 1-2 times ,Heating temp 120 degree
HD silicone XG-866A 50%
Elastic silicone XG-866A-LK 50%
Catalyst XG-866B-2 2%
Pigment 10%
3.Pulling stone printing for 1 time more thinner can be easy pulling ,Enough silicone for coating
HD silicone XG-866A 50%
Elastic silicone XG-866A-LK 50%
Catalyst XG-866B-2 2%
Thinner XG-128AH 20-30%