Mesh number 80-120 (32-48T)
Embossing printing silicone ink and catalyst Mixing Ratio:Embossing silicone ink XG-360KY-55:50GEmbos sing silicone catalyst XG-360BH:5G(mixing ratio 10%)Silicone thinner XG-128AH:not necessary
Print mixing silicone ink on the backside of the fabric
Machine temp set temp:
Upper mold 180 degree Bottom mold 120-150 degree
Can stick a thin fabric on the printing fabric backside(depends on design)Heating time 8-15 seconds (depends on temp and design size)